Nanoindentation for professionals

In material testing, the dynamic method has increasingly come to complement classic nanoindentation. Analogous to dynamic-mechanical analysis (DMA), it allows testing of the visco-elastic properties of substances. The Helmut Fischer FISCHERSCOPE® HM2000 determines properties such as the indentation hardness and the depth-dependent elastic modulus – and all of that in the nanometer range!

If you want to measure a sample in multiple places or do automated testing, the FISCHERSCOPE HM2000 is ideal. In just a few clicks, you can program in the measuring points  – the instrument takes care of the rest.

In addition to quality testing in electroplating, a common area of application for the FISCHERSCOPE HM2000 is the characterization of polymers at different temperatures. For this purpose, the automated system can be equipped with a heating stage.

Download pdf brochure here: Microhardness Product Line Measurement System for the Instrumented Indentation Test

Features

  • Determination of the material parameters according to DIN EN ISO 14577-1 Annex A and ASTM E 2546
  • Dynamic mode for determining viscoelastic material properties (dynamic mechanical analysis)
  • Fast measurement: the zero point is determined within 30 seconds
  • Only minimal sample preparation required, even on dark surfaces
  • Suitable for testing solid materials and coatings > 1 µm thick, test-force range 0.1 – 2000 mN 
  • Thermally stable and resistant to vibrations: measures for several hours without external influences
  • Programmable sample stage for automated testing of multiple measurement points
  • Microscope with magnification levels from 4x to 40x for exact positioning of the measuring spot
  • Modular design enables customer-specific configurations or future upgrades of the device
  • Indenters: Vickers, Berkovich, carbide ball, Knoop or customized indenters
  • Powerful WIN-HCU software for intuitive operation and evaluation 

Applications

  • Measurement of the hardness and elasticity of paint layers, for example automotive paint finishes
  • Testing of anodized layers
  • Instrumented indentation testing of hard material coatings, e. g. on tools
  • Characterization of surfaces in research and development, for example hard chrome or ceramic coatings on medical implants
  • Series testing in electroplating
  • Quality assurance of circuit boards, e. g. testing thin gold coatings or insulating layers 
  • Hardness testing on complex-shaped parts like housings
  • Characterization of composite materials

 